Elk Battery Lifeer Blt Users Manual V2 Instructions
BLT to the manual ed884ed6-b56c-4e5c-a299-45dec8660b43
2015-02-06
: Elk Elk-Battery-Lifeer-Blt-Users-Manual-539701 elk-battery-lifeer-blt-users-manual-539701 elk pdf
Open the PDF directly: View PDF .
Page Count: 4
Battery LifeTester
ELK-BLT v.2 Mhos Meter
PO Box 100 • Hildebran, NC 28637 • 800-797-9355 • 828-397-4200
Fax 828-397-4415 • www.elkproducts.com • info@elkproducts.com
Features
The NEW and improved ELK-BLT v.2 Battery
LifeTester is a compact, easy to use Mhos Meter for
testing 12 Volt rechargeable batteries. Unlike ordinary
testers which only measure static criteria, the LifeTester
measures internal conductivity, which is the best
indicator of a battery’s health and life expectancy. The
conductivity value, expressed in Mhos (the inverse of
Ohms or resistance), is easily compared to benchmark
readings from the included Mhos Chart. The chart then
categorizes the battery condition as “Best, Good, Weak,
or Bad”. Every battery type has a characteristic Mhos
value when it is brand new and fully charged.
The LifeTester is powered by the battery under test and
automatically warns when the battery voltage is too low
for testing.
Specifications
• Operating Voltage: 10.0V - 14 Volts D.C.
• Current Draw: 1.1 Amps Max., 0.0016 Ah for full test.
• Battery Leads: ~12 Inches.
• Size: 4.4” W x 3”H x 1.15”D w/o carrying case.
ELK
PRODUCTS, INC.
** To reorder a pack of 100 test data labels specify: ELK-BLT LABELS.
• Does not discharge or damage the battery.
• Tests 12 Volt Rechargeable Batteries.
• Display Shows Battery Voltage and Mhos.
• Warns if battery voltage is too low.
• Replaceable test leads.
• Includes padded carrying case.
• Includes self-adhesive test data labels. **
• Lifetime Limited Warranty.
05/04
Instructions ELK - BLT
1. Disconnect the battery from it’s equipment.
2. Connect the BLACK test clip to the Negative (-) battery terminal, and the RED to the Positive (+) terminal. (For accurate
readings, the test clips must be tightly clipped directly to the battery posts, not to the battery bolts).
“Err” or blank indicates battery voltage is too low for testing or a test clip connection is loose.
Try charging the battery or reconnecting the test clips.
3. The Voltage of the Battery will display briefly. A new battery, out of the box, will generally read around 12.6 Volts. A fully-
charged battery should read between 12.6 Volts and 13.5 Volts.
“- - -” indicates test in process, please wait.
4. The Mhos (internal conductance) reading of the battery will display within 6 seconds.
5. Refer to the Mhos Chart. In the Ah column, find the battery size. Follow across the row to find the closest match to it’s Mhos
reading. The column heading and color code indicates the test results.
NOTE: The Mhos chart printed on the BLT is best suited for batteries under charge and at room temperatures of
around 72F degrees. This covers most batteries, even in cold basements or buildings, since the battery will be kept
warm by the recharging and by being inside the electronics enclosure. However, since cooler temperatures can
significantly lower the Mhos reading of a battery, this instruction manual has a more extensive Mhos chart with
columns for evaluating batteries that are being adversely affected by 62F, 52F, and 42F degree environments. Also
see How Temperature affects a Battery
6. For future reference mark the battery with the Voltage, Mhos reading, and test date.
Automatic Shutdown
If the LifeTester is left connected to a battery for more than 30 seconds after the test is complete, it will automatically shutdown to
conserve battery power. Disconnecting and reconnecting a test lead will restart the test procedure.
Recording Battery Readings
LifeTester measurements should be taken and recorded periodically. The popular method is to record the information onto self-
adhesive labels placed directly onto the battery. A supply of these labels is included with the tester. Additional labels may be
ordered in packs of 100 by specifying part number ELK-BLT LABELS. This information will be valuable in future tests for trending
analysis. The recorded data should include:
A. The Date of the test.
B. The Battery Voltage reading. (optional)
C. The Mhos reading.
A new “fresh out of the box” battery that has not been charged should have a Mhos value in the high side of the Good column and
quite possibly into the Best column. See the Mhos chart. If the reading is considerably lower, charge the battery for at least 24
hours and then retest.
Battery performance degrades over time due to use and abuse, and may be impacted by many factors like depth and frequency of
discharge. The higher the Mhos value the more current the battery can deliver. Therefore, a new 7 amp-hour battery will have a
higher Mhos value than a new 4 amp-hour battery of the similar construction.
Instructions ELK - BLT
How Temperature affects a Battery
Generally speaking, temperatures below 72F degrees tend to slow down a battery’s internal activity, causing a significant decrease
in the Mhos (conductivity) reading as the temperature falls. Cool temperatures (not below freezing) will tend to prolong a battery’s
life. Temperatures above 72F cause a battery’s internal activity to accelerate, but with only a slight increase in the Mhos reading.
Warm temperatures will tend to dry out and degrade a battery much faster than normal.
100 F degrees = 105 % of normal Mhos (conductivity) 52 F degrees = 87 % of normal Mhos (conductivity)
72 F degrees = 0 % no adjustment 42 F degrees = 82 % of normal Mhos (conductivity)
62 F degrees = 92 % of normal Mhos (conductivity) 32 F degrees = 76 % of normal Mhos (conductivity)
ELK Products is not responsible for misprints or errors. These Mhos values are benchmark averages, created from fresh samples of major brand batteries. If you find consistent,
minor variations in readings from multiple samples of a battery, it’s likely due to manufacturing differences. However, if the readings are excessively low, the battery is not as good
as the benchmark average. If this chart does not include the battery you are testing, it may be necessary to generate the values using the procedure below.
Adding to the Battery Mhos Chart
If the battery you are trying to test is not included in the Battery Mhos Chart it may be necessary to research and generate the
data on your own. The following procedure will help with this task.
Start with 2 or 3 fresh new batteries out of the box. The battery voltage should be around 12.6 Volts or higher. Place the batteries
in service (on charge) for 24 hours. Remove them from charge and measure the Mhos reading of each one. Average the readings
together. This will be the baseline number from which the Best, Good, Weak, and Bad columns are calculated. The “Best” column
will be 90% of the baseline number. The first and second numbers in the “Good” column are 80% and 89% of the baseline. The first
and second numbers in the “Weak” column are 70% and 79% of the baseline. The “Bad” column is 0% and 69% of the baseline.
Accumulating Trend Analysis over a Period of Years
Trending of periodic Mhos measurements can yield valuable insights for estimating the remaining life of the battery. Suppose that
a 4.0 Ah battery has been in service for three years and that the LifeTester measurements after the first year was 90 Mhos, 85 Mhos
after the second year, and 80 Mhos after the third year. Since the battery is still at 80 Mhos and is dropping an average of 5 Mhos
per year, it is highly likely that this battery will not need replacing before the end of the fourth year. On the other hand, suppose that
the readings were 90 Mhos after the first year, 82 Mhos after the second year, and 70 Mhos after the third year. The rate of decay
has increased from 8 Mhos to 12 Mhos per year. This indicates that although the battery is still serviceable, it is degrading more
and more rapidly. It is unlikely that this battery will be serviceable for another year. Under these circumstances, either the battery
should be replaced early or the service interval should be shortened to catch this battery before a system failure.
Why Mhos instead of Amp Hour
The LifeTester measures the Mhos (conductance) of a battery using an AC impedance measurement algorithm. Every battery
manufacturing process produces a slightly different conductance value for a given battery size. Elk Products elected to display
consistent, accurate Mhos (conductance) values, rather than just estimated Amp Hour values. The only accurate method for
measuring a battery’s Amp-hour capacity is with a long discharge test, which actually decreases the life of the battery. Estimation
of Amp-hour capacity without a discharge test is a complex error-prone process involving the conductance value, the battery state-
of-charge, the voltage, the temperature, and the many varying design and production variables for each battery type. Ordinary
testers which measure static criteria or Amp-hour are inherently inaccurate across varying battery designs. In contrast, extensive
testing has proven that when the conductance of a charged battery is tested and has declined to approximately 70% of its full-
capacity reference, the battery is unlikely to deliver its rated capacity and should be replaced.
Is Mhos relational to Cold Cranking Amp
The LifeTester is designed to measure the conductance of a battery at frequencies indicative of the capacity of a battery in Amp-
hour. Conductance measurements for estimating the Cold Cranking Amps for starter type batteries are at a much higher frequency.
Although the measurement techniques are similar, there is little correlation between the Cold Cranking Amps measurement of a
battery and the Mhos reading of the LifeTester, or vice-versa.
Using Mhos to Estimate Battery Life
The Mhos reading of a new battery out of the box, will generally not be the same as that of a fully charged battery. This is due to
the plates not being totally formed during manufacturing. Once the battery has been on charge for some time the plates will finish
forming and the peak Mhos reading will normalize. For standby batteries, peak capacity is normally reached after about three
months on a float charging system. For cyclic use batteries, full capacity may not be reached until after ten to thirty cycles,
depending upon the depth of discharge and the charging method.
If a new battery has been in storage for an extended period, say over six months without being charged, plate oxidation from self-
discharge will occur, causing a decrease in the Mhos reading. Plate oxidation also occurs in standby batteries during a power
failure, particularly if a battery remains in a highly discharged state for an extended time period. Plate oxidation is unhealthy and
can destroy a battery’s capacity. Once a battery is weakened by plate oxidation, it is difficult to recover full capacity without special
charging or conditioning methods. In some cases a battery will recover and pass a test after being recharged. However, a second
test should be performed a few days later after recovery to accurately assess the overall life of the battery.
The average life cycle of a sealed lead-acid battery in standby use on a float charge is 3 to 5 years. A battery with a Mhos reading
of less than 70% of its original capacity is no longer considered serviceable and should be replaced.